Nickel and high-performance alloys

Nickel alloys are chosen when stainless steel is not enough: very high temperatures, aggressive chemicals or seawater. The family includes nickel-chromium superalloys (625, 718), nickel-copper alloys (400, K-500), nickel-molybdenum alloys (C-276) and controlled-expansion alloys (Invar 36, Kovar).

They are expensive and among the slowest materials to machine, so quotes should account for long cycle times and tool wear. Trade names belong to their owners; UNS numbers are the neutral way to specify them.

Price drivers

Data through Oct 2026 · updated monthly
Nickel · monthly average · USD per metric ton
$15,436
▼ 5.4% vs Sep 2026
$14,423$15,581$16,739$17,896$19,054Oct 2025Dec 2025Feb 2026Apr 2026Jun 2026Aug 2026Oct 2026High $18,806Low $14,671
$13,516$18,907$24,298$29,688$35,079Oct 2021Jul 2022Apr 2023Jan 2024Oct 2024Jul 2025Apr 2026High $33,924Low $14,671
$-774$10,450$21,675$32,900$44,1241960196919791989199820082018High $41,719Low $1,631
Latest (monthly avg)
$15,436
Oct 2026
1-month change
−5.4%
1-year change
+2.3%
5-year change
−20.3%
12-month high
$18,806
May 2026
12-month low
$14,671
Nov 2025
12-month average
$16,758
Year to date
+3.7%
5-year high
$33,924
Mar 2022
5-year low
$14,671
Nov 2025
Record monthly high
$52,179
May 2007
Volatility (5Y, ann.)
29.4%
std. dev. of monthly moves
Nickel statistics
Latest$15,436
MonthOct 2026
1-month change−5.4%
1-year change+2.3%
5-year change−20.3%
12-month high$18,806
12-month low$14,671
Nickel$/t
$15,436
USD per metric ton · World Bank monthly average
1M ▼ 5.4%1Y ▲ 2.3%5Y ▼ 20.3%
5-year monthly · Oct 2026
12M low $14,67112M high $18,806
Nickel & nickel-base alloy mill shapesIndex
232.8
BLS PPI WPU102504 · index, base period = 100
1M ▼ 0.7%1Y ▲ 10.5%5Y ▲ 27.0%
5-year monthly · Oct 2026
12M low 209.612M high 235.3

How to choose

625 for corrosion and weldability, 718 for high strength at temperature, 400 or K-500 for seawater, C-276 for severe chemicals, 600 or 800 for furnace parts and Invar 36 or Kovar for thermal-expansion matching.

Material grades

Difficult

Nickel 200

UNS N02200, commercially pure wrought nickel (99.0% min)

Difficult

Inconel 600 (UNS N06600)

UNS N06600 nickel-chromium-iron alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Inconel 625 (UNS N06625)

UNS N06625 nickel-chromium-molybdenum-niobium alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Inconel 718 (UNS N07718)

UNS N07718 precipitation-hardening nickel-chromium alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Inconel X-750 (UNS N07750)

UNS N07750 precipitation-hardening nickel-chromium alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Monel 400 (UNS N04400)

UNS N04400 nickel-copper alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Monel K-500 (UNS N05500)

UNS N05500 age-hardenable nickel-copper alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Hastelloy C-276 (UNS N10276)

UNS N10276 nickel-molybdenum-chromium alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Hastelloy X (UNS N06002)

UNS N06002 nickel-chromium-iron-molybdenum alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Waspaloy (UNS N07001)

UNS N07001 precipitation-hardening nickel superalloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Difficult

Invar 36 (UNS K93600)

UNS K93600 / K93603, 36% nickel-iron controlled-expansion alloy (Invar is a trade name of its owner)

Difficult

Kovar (ASTM F15)

ASTM F15 (UNS K94610) iron-nickel-cobalt sealing alloy (Kovar is a trade name of its owner)

Difficult

Alloy 20 (UNS N08020)

UNS N08020 nickel-iron-chromium alloy with copper and molybdenum (Carpenter 20 is a trade name of its owner)

Difficult

Incoloy 800 (UNS N08800)

UNS N08800 iron-nickel-chromium alloy. Trade names such as Inconel, Monel, Hastelloy and Waspaloy belong to their owners; the UNS number is the neutral way to specify the alloy.

Common manufacturing processes

  • CNC milling
  • CNC turning
  • Wire EDM
  • Waterjet and laser cutting
  • TIG welding

Finishing options

  • As machined
  • Passivation / pickling
  • Bead blasting
  • Electropolishing

Suppliers

Find shops

Frequently asked questions

Which nickel and high-performance alloys grade should I choose?

625 for corrosion and weldability, 718 for high strength at temperature, 400 or K-500 for seawater, C-276 for severe chemicals, 600 or 800 for furnace parts and Invar 36 or Kovar for thermal-expansion matching.

Which nickel and high-performance alloys grades does this library cover?

Nickel 200, Inconel 600 (UNS N06600), Inconel 625 (UNS N06625), Inconel 718 (UNS N07718), Inconel X-750 (UNS N07750), Monel 400 (UNS N04400), Monel K-500 (UNS N05500), Hastelloy C-276 (UNS N10276), Hastelloy X (UNS N06002), Waspaloy (UNS N07001), Invar 36 (UNS K93600), Kovar (ASTM F15), Alloy 20 (UNS N08020), Incoloy 800 (UNS N08800).